ITI Interview Q&A – Traditional Crafts Trades
ITI Interview – Traditional Crafts Trades — 7 trades, 140 interview questions. Click a trade to see its 20 Q&A. Bamboo Works 20 Q&A Q1. What does the Bamboo Works trade cover? It covers techniques for crafting furniture, baskets, decorative items, and utility products using bamboo as the primary raw material, including cutting, shaping, and finishing processes. Q2. What is the difference between raw bamboo and treated bamboo? Raw bamboo is untreated and prone to insect attack and decay, while treated bamboo undergoes processes like boiling, chemical treatment, or smoking to improve durability and lifespan. Q3. What tools are commonly used in bamboo craft work? Saws, knives, chisels, and specialized bamboo splitting tools are commonly used to cut, shape, and join bamboo pieces into finished products. Q4. What is the importance of selecting mature bamboo for craft production? Mature bamboo is stronger and more durable than young bamboo, making it more suitable for p...